Increase of corrossion resistance of nickel-based superalloys in contact with molten salts by combined heat and mechanical treatment

Increase of corrossion resistance of nickel-based superalloys in contact with molten salts by combined heat and mechanical treatment / A. Yu. Zhlyakov, A. V. Abramov, V. V. Karpov [et al.] // 16th IUPAC Conference on High Temperature Materials Chemistry (HTMC-XVI), July 2-6, 2018, Ekaterinburg, Russia. - Ekaterinburg, 2018. - P. 201.